Wear of primary teeth caused by opposed all-ceramic or stainless steel crowns
Authors:Jae-Won Choi  Ik-Hyun Bae  Tae-Hwan Noh  Sung-Won Ju  Tae-Kyoung Lee  Jin-Soo Ahn  Tae-Sung Jeong  Jung-Bo Huh
Abstract:

PURPOSE

This study was conducted to evaluate the effects of full-coverage all-ceramic zirconia, lithium disilicate glass-ceramic, leucite glass-ceramic, or stainless steel crowns on antagonistic primary tooth wear.

MATERIALS AND METHODS

There were four study groups: the stainless steel (Steel) group, the leucite glass-ceramic (Leucite) group, the lithium disilicate glass-ceramic (Lithium) group, and the monolithic zirconia (Zirconia) group. Ten flat crown specimens were prepared per group; opposing teeth were prepared using primary canines. A wear test was conducted over 100,000 chewing cycles using a dual-axis chewing simulator and a 50 N masticating force, and wear losses of antagonistic teeth and restorative materials were calculated using a three-dimensional profiling system and an electronic scale, respectively. Statistical significance was determined using One-way ANOVA and Tukey''s test (P<.05).

RESULTS

The Leucite group (2.670±1.471 mm3) showed the greatest amount of antagonist tooth wear, followed by in decreasing order by the Lithium (2.042±0.696 mm3), Zirconia (1.426±0.477 mm3), and Steel groups (0.397±0.192 mm3). Mean volume losses in the Leucite and Lithium groups were significantly greater than in the Steel group (P<.05). No significant difference was observed between mean volume losses in the Zirconia and Steel groups (P>.05).

CONCLUSION

Leucite glass-ceramic and lithium disilicate glass-ceramic cause more primary tooth wear than stainless steel or zirconia.
Keywords:Leucite porcelain  Lithium disilicate porcelain  Zirconia  Primary tooth  Wear