Shear bond strength between metal alloy and a ceramic system, submitted to different thermocycling immersion times
Authors:Salazar M Susana M  Pereira Sarina M B  Ccahuana V Vanessa Z  Passos Sheila P  Vanderlei Aleska D  Pavanelli Carlos A  Bottino Marco A
Affiliation:Department of Dental Materials and Prostheses, Paulista State University, S?o José dos Campos, Brazil. susana_works@yahoo.com.br
Abstract:The aim of this study was to evaluate the shear bond strength of Co-Cr and Ni-Cr metal alloys and a specific ceramic, submitted to different thermocycling immersion times. Sixty metal-ceramic specimens were confectioned and standardized in cylindricalformat. Three thermocycling conditions were evaluated: without thermocycling, 3,000 cycles (5 degrees C/55 degrees C+/-1) with 30s of immersion time and 3,000 cycles (5 degrees C/55 degrees C+/-1) with 60s. The shear bond strength was performed in a universal testing machine, using a special device to concentrate the tension at the metal/ceramic interface during the test. The load was applied until fracture of the specimens. The data was statistically analyzed by ANOVA (two-way) and Tukey (p<0.05) test. The results didn't show significant statistic differences between the metal-porcelain combinations. Nevertheless, both metal-ceramic systems submitted to 60s of immersion time showed lower values compared to specimens without thermocycling. It was concluded that the thermocycling immersion time of 1 minute affect the shear bond strength values for the Ni-Cr/porcelain and Cr-Co/porcelain systems.
Keywords:
本文献已被 PubMed 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号