Adhesive bonding of titanium with a titanate coupler and 4-META/MMA-TBB opaque resin |
| |
Authors: | H Matsumura K Yoshida T Tanaka M Atsuta |
| |
Affiliation: | Department of Fixed Prosthodontics, Nagasaki University School of Dentistry, Japan. |
| |
Abstract: | Adhesive bonding of titanium was evaluated with a titanate primer and adhesive opaque resin. The primer consisted of 2% isopropyl dimethacryloyl isostearoyl titanate in methyl methacrylate. The adhesive was 4-META/MMA-TBB opaque resin that contained 4-methacryloyloxyethyl trimellitate anhydride and was initiated by tri-n-butylborane derivative. Titanium discs were machined and blasted with aluminum oxide. They were primed and bonded together with the opaque resin. A shear test was performed after repeated thermocycles for investigation of the durability of the bond. The shear strength of the primed and 4-META resin-bonded specimens was 37.2 MPa after 50,000 thermocycles, with only a small decrease in bond strength. This was significantly higher than the control values. Thus, titanate primer and 4-META/MMA-TBB opaque resin may be used for the bonding of titanium in prosthodontic practice. |
| |
Keywords: | |
|
|