Evaluation of the adaptation of complete denture metal bases fabricated with dental CAD-CAM systems: An in vitro study
Authors:Seung-Gyu You  Seung-Min You  Seen-Young Kang  So-Yeon Bae  Ji-Hwan Kim
Affiliation:1. Doctoral student, Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University, Seoul, Republic of Korea;2. Doctoral student, Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University, Seoul, Republic of Korea;3. Researcher, Medical Device Research Division, National Institute of Food and Drug Safety Evaluation, Osong, Republic of Korea;4. Doctoral student, Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University, Seoul, Republic of Korea;5. Professor, Department of Dental Laboratory Science and Engineering, College of Health Science, Korea University, Seoul, Republic of Korea
Abstract:Statement of problemConventional fabrication of complete denture metal bases is being replaced by the computer-aided design and computer-aided manufacturing (CAD-CAM) systems. However, a comparative analysis of subtractive and additive CAD-CAM manufacturing techniques is lacking.PurposeThe purpose of this in vitro study was to compare the adaptation of complete denture metal bases fabricated by milling (subtractive manufacturing) and stereolithography apparatus (SLA) and digital light processing (DLP) (additive manufacturing).Material and methodsThirty metal bases were manufactured by using the milling (MIL group), SLA (SLA group), and DLP (DLP group) techniques. The silicone replica technique was used to evaluate the adaptation of the complete denture metal bases, and 30 silicone blocks were fabricated. The silicone block was cut equally in the canine, first molar, and second molar areas. The gap between the model and the metal base was measured by using a digital microscope at the 3 locations, and the measured data were statistically analyzed by using a statistical software program (α=.05).ResultsThe gaps measured at the 3 areas showed significant differences in all 3 groups (P<.05). At the anterior, middle, and posterior areas, the SLA group showed the narrowest gap (302 ±31 μm, 241 ±39 μm, 201 ±43 μm, respectively). The SLA group also had the narrowest total gap of the metal bases (218 ±33 μm).ConclusionsThe adaptation of the fabricated metal bases varied significantly across the techniques used but fell within a clinically allowable range. The SLA group was the most precise in the fabrication of complete denture metal bases. Further studies are required to analyze the effects of the layer thickness setting, wax elimination, and casting temperature on the adaptation of metal bases manufactured by using SLA.
Keywords:
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号