Fracture resistance of endodontically treated maxillary premolars restored by silorane-based composite with or without fiber or nano-ionomer
Authors:Fereshteh Shafiei  Maryam Sadat Tavangar  Yasamin Ghahramani  Zahra Fattah
Institution:1.Department of Operative Dentistry, School of Dentistry, Shiraz University of Medical Sciences, Shiraz, Iran.;2.Biomaterial Research Center, School of Dentistry, Shiraz University of Medical Sciences, Shiraz, Iran.;3.Department of Endodontics, School of Dentistry, Shiraz University of Medical Sciences, Shiraz, Iran.
Abstract:
Keywords:Endodontically treated premolar  Intracoronal direct restoration  Silorane-based composite  Polyethylene fiber  Nano-ionomer  Fracture resistance