Microshear bond strength of dual-cure resin cement in zirconia after different cleaning techniques: an in vitro study
Authors:Katherine Joselyn Atoche-Socola,Luis Ernesto Arriola-Guillé  n,Ana Isabel Ló  pez-Flores,Isadora Martini Garcia,Gustavo Huertas-Mogolló  n,Fabrí  cio Mezzomo Collares,Vicente Castelo Branco Leitune
Affiliation:1.Division of Oral Rehabilitation, School of Dentistry, Universidad Científica Del Sur, Lima, Perú.;2.Division of Orthodontic, School of Dentistry, Universidad Científica Del Sur, Lima, Perú.;3.Dental Materials Laboratory, School of Dentistry, Federal University of Rio Grande do Sul, Ramiro Barcelos, Rio Branco, Porto Alegre, RS, Brazil.
Abstract:PURPOSEThis study aimed to compare the microshear bond strength (µSBS) of dual-cure resin cement in CAD-CAM zirconia after different cleaning techniques.MATERIALS AND METHODSFifty discs of zirconia-based ceramic from Ivoclar Vivadent were embedded in acrylic resin. The discs were divided into five groups according to the cleaning methods used: Group 1: drying with spraying + sandblasting with Al2O3; Group 2: washed with water and dried with spraying + sandblasting with Al2O3; Group 3: washed with distilled water and dried with spraying + sandblasting with Al2O3 + zirconium oxide (Ivoclean); Group 4: washed with distilled water and dried with spraying + sandblasting with Al2O3 + potassium hydroxide (Zirclean); and Group 5: washed with distilled water and dried with spraying + sandblasting with Al2O3 + 1% NaClO. All of the groups were contaminated with artificial saliva for 1 minute and then cleaned. Statistical analyses were performed using ANOVA and Tukey''s tests. RESULTSThere were statistically significant differences among all groups for µSBS (P < .05). The group treated with zirconium oxide (Group 3) showed the highest µSBS (18.75 ± 0.23 MPa).CONCLUSIONWhen applied to zirconia, the cleaning methods affected the bonding with resin cement differently.
Keywords:Zirconia   Ceramics   Dental cements   Cleaning   Mechanical test