首页 | 本学科首页   官方微博 | 高级检索  
检索        

不同品牌光固化树脂材料颜色稳定性评价
引用本文:朱晔,谢海峰,光寒冰,王瑜,章非敏.不同品牌光固化树脂材料颜色稳定性评价[J].口腔医学,2009,29(3):119-121.
作者姓名:朱晔  谢海峰  光寒冰  王瑜  章非敏
作者单位:南京医科大学口腔医学研究所,南京医科大学附属口腔医学院修复科,南京,210029
基金项目:江苏省兴卫工程重点人才项目 
摘    要:目的探讨紫外线对几种树脂基材料老化颜色的影响。方法制作树脂试件5枚/组(A组,Biscem;B组,PermaCem;C组,Choice;D组,Elite Flo;E组,Clearfil AP-X;F组,Dyract extra;G组,Durafill VS;H组,Filtek Z350Universal)。在黑暗环境保持24h后用色度计测量颜色值CIE L*、a*、b*,随后各组试件分别在紫外线照射老化8h、16h、24h再次测量,对结果进行统计分析。结果照射后试件均显示了一定程度的颜色值变化,树脂水门汀色差值变化范围从8h内的2.31~2.60到24h时的3.27~7.19,树脂充填材料色差值变化范围从8h内的1.35~2.66到24h时的3.36~14.31。其中,PermaCem、Durafill VS、FiltekZ350Universal24h后出现较大的色差值,其余组间无明显差异。结论紫外线老化能够引起树脂基材料发生颜色改变,除PermaCem、Durafill VS、Filtek Z350Universal同类产品不同品牌的颜色稳定性24h后无明显差异。

关 键 词:树脂  颜色  紫外线老化

Color variations in different resin-based composite products after UV irradiation
ZHU Ye,XIE Hai-feng,GUANG Han-bing,WANG Yu,ZHANG Fei-min.Color variations in different resin-based composite products after UV irradiation[J].Stomatology,2009,29(3):119-121.
Authors:ZHU Ye  XIE Hai-feng  GUANG Han-bing  WANG Yu  ZHANG Fei-min
Institution:. ( The Research Institute of Stomatology , Department of Prosthodontics,School of Stomatology, Nanfing Medical University, Nanjing 210029, China)
Abstract:Objective To investigate the color stability of eightresin-bused composite products after UV nging.Methods 40 discs for eight groups(Group A, Biscem; Group B, PermaCem; Group C, Choice; Group D, Elite Flo; Group E, Clearfil AP-X; Group F, Dyraet extra; Group G, Durafill VS;Group H, Filtek Z350 Universal) were prepared. Changes in color of test samples were determined before and after UV aging for 8, 16 and 24 hours using the CIE-Lab system by a colorimeter. The results were analyzed by one-way ANOVA. Results The color change of composite disks suffering UV aging was significantly different due to irradiated different time. Color difference values among the resin cement groups ranged from 1.85 -2.60 for 8 hours to 2.88- 4.55 for 24 hours. The values among composite resin ranged from 1.35 - 2.66 for 8 hours to 3.36 -14.31 for 24 hours. PermaCem, Durafill VS and Fihek Z350 Universal showed the biggest color change, while difference was found between other groups. Conclusions It can be concluded that for some products, UV irradiation leads to color instability. It's different between groups.
Keywords:resin  color  UV aging
本文献已被 维普 万方数据 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号