Composite-to-composite microtensile bond strength in the repair of a microfilled hybrid resin: effect of surface treatment and oxygen inhibition |
| |
Authors: | Papacchini Federica Dall'Oca Susanna Chieffi Nicoletta Goracci Cecilia Sadek Fernanda Tranchesi Suh Byoung I Tay Franklin R Ferrari Marco |
| |
Affiliation: | Department of Dental Materials and Restorative Dentistry, University of Siena, Policlinico "Le Scotte" Viale Bracci, Siena, Italy. |
| |
Abstract: | PURPOSE: To compare the 24-h microtensile bond strength of a microfilled hybrid composite to the same material after mechanical and/or chemical treatment and assess the effect of oxygen inhibition on the composite-composite bond. MATERIALS AND METHODS: Forty composite cylinders of Gradia Direct Anterior (GC) were prepared and stored 24 h prior to the following surface treatments: 50-microm aluminum oxide air abrasion and 37% phosphoric acid etching (group 1); hydrochloric acid and 6.9% hydrofluoric acid etching (group 2); diamond bur roughening and 37% phosphoric acid etching (group 3); diamond bur roughening (group 4). In all groups, Prime & Bond NT (Dentsply De Trey) was applied and light cured in air or under a nitrogen atmosphere, prior to layering a buildup of the repairing resin composite. Microtensile bond strength measurements were performed. Data were statistically analyzed with two-way ANOVA and Tukey's test (alpha = 0.05). RESULTS: The curing atmosphere did not significantly influence the interfacial strength (p < 0.05). Surface treatment significantly affected the composite-composite bond (p > 0.05). Air abrasion, regardless of curing atmosphere, resulted in the strongest bond (p < 0.05). The other treatments were comparable. CONCLUSION: Air abrasion and the application of a bonding agent offer satisfactory bond strengths for composite repair. The oxygen inhibition layer on a light-cured adhesive is not crucial to the success of the 24-h composite-composite bond. |
| |
Keywords: | |
本文献已被 PubMed 等数据库收录! |
|