Block Copolymers of Methyl Vinyl Ether and Isobutyl Vinyl Ether With Thermo‐Adjustable Amphiphilic Properties
Authors:Beatrice Verdonck  Eric J Goethals  Filip E Du Prez
Abstract:The thermo‐adjustable hydrophilic/hydrophobic properties of AB, ABA and BAB block copolymers in which A is poly(methyl vinyl ether) (PMVE) and B is poly(isobutyl vinyl ether) (PIBVE) have been investigated. The block copolymers were prepared by “living” cationic polymerization using sequential addition of monomers. The polymerizations were carried out with the system acetal/trimethylsilyl iodide as initiator and ZnI2 as activator. The initiating system based on diethoxyethane leads to AB block copolymers whereas the initiating system based on tetramethoxypropane leads to ABA or BAB triblock copolymers. Well‐defined block copolymers of different composition with controlled molecular weights up to approx. 10 000 have been prepared. When IBVE is added to living PMVE, PIBVE‐blocks form only in the presence of an additional amount of ZnI2, which is attributed to the fact that part of the ZnI2 is inactive because of complex formation with PMVE. At room temperature, the combination of hydrophilic (PMVE) and hydrophobic (PIBVE) segments provides the copolymers with surfactant properties. Above the lower critical solution temperature (LCST) of PMVE, situated around 36 °C, the PMVE‐blocks become hydrophobic and the amphiphilic nature of the block copolymers is lost. The corresponding changes in hydrophilic/hydrophobic balance have been evaluated by investigation of the emulsifying properties of the block copolymers for water/decane mixtures as a function of the temperature. Below the LCST, the block copolymers have emulsifying properties similar to or better than those of the commercial PEO‐PPO block copolymers (Pluronic®). Either oil‐in‐water or water‐in‐oil emulsions can be obtained, depending on the polymer architecture and the water/decane volume ratio. The emulsifying properties are strongly reduced or completely lost above 40 °C. Emulsions obtained with a PMVE36b‐PIBVE54 block copolymer for a water/decane (v/v) ratio of 85/15 remained stable for more than six months.
image

50/50 and a 85/15 water/decane w/o emulsion (15 g/l) with the PMVE36b‐PIBVE54 block copolymer at 20 °C.

Keywords:amphiphiles  emulsions  living cationic polymerization  lower critical solution temperature  poly(vinyl ether)  thermo‐responsive
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号