Mixing with Propylene Glycol Enhances the Bond Strength of Mineral Trioxide Aggregate to Dentin |
| |
Authors: | Amin Salem Milani Mohammad Froughreyhani Saeed Charchi Aghdam Fatemeh Pournaghiazar Mohammad Asghari Jafarabadi |
| |
Affiliation: | 1. Dental and Periodontal Research Center, Tabriz University of Medical Sciences, Tabriz, Iran;2. Department of Endodontics, Faculty of Dentistry, Tabriz University of Medical Sciences, Tabriz, Iran;3. Department of Operative Dentistry, Faculty of Dentistry, Tabriz University of Medical Sciences, Tabriz, Iran;4. Department of Statistics and Epidemiology, Faculty of Dentistry, Tabriz University of Medical Sciences, Tabriz, Iran |
| |
Abstract: | IntroductionMixing mineral trioxide aggregate (MTA) with different proportions of propylene glycol (PG) improves its handling property. The aim of this study was to evaluate the effect of PG on MTA-dentin push-out bond strength.MethodsSeventy-five 2-mm-thick midroot sections were prepared from single-rooted human extracted teeth. The lumen of each slice was enlarged with Gates-Glidden burs. The slices were randomly divided into 3 groups (n = 25). In each group, 0.3 mL of the liquid was mixed with 1 g MTA (Angelus, Londrina, Brazil). The liquid vehicles used in groups 1–3 were 100% distilled water (DW), 20% PG–80% DW, and 100% PG, respectively. After incubation, the push-out strength of the samples was measured using a universal testing machine. The samples were then cut in halves and examined under a stereomicroscope to determine the failure pattern. One-way analysis of variance followed by the Tukey post hoc test was used to compare the push-out strength among groups.ResultsThere were statistically significant differences between groups (P < .001). The push-out strength in group 1 (DW) was significantly lower than groups 2 and 3 (P < .001 and P = .022, respectively). However, there was no significant difference between groups 2 (DW-PG) and 3 (PG).ConclusionsMixing MTA with PG increased its push-out bond strength to dentin. In the present study, the most suitable ratio was 80% DW–20% PG. |
| |
Keywords: | Mineral trioxide aggregate propylene glycol push-out strength |
本文献已被 ScienceDirect 等数据库收录! |
|