Abstract: | A new series of polyimides was synthesized by addition polymerization of 4,4′-(bismaleimido)-diphenylmethane, 1,4-piperazine and an amino-terminated polydimethylsiloxane. The synthesis was carried out in m-cresol solution following a two-step procedure. Copolymers containing 15 and 20 wt.-% of the polydimethylsiloxane elastomer were prepared, together with the unmodified base copolymer. Infrared spectroscopy, 13C and 1H NMR, thermal and thermogravimetric analyses were used to characterize the copolymers. The DSC curves of all the samples showed an exotherm in the temperature range 230–280°C, attributable to curing and addition reactions involving the chain-end groups. Different glass transition temperatures (Tg) were observed, depending on the elastomer content. Thermogravimetric analysis indicated that no significant changes occur in the thermal stability of rubber-modified copolymers. |